Abstract
The properties of a composite material depend on fibres, matrix and interface properties. In order to study the ceramic composites SiC-SiC we characterized some commercial (Nicalon) silicon carbide fibres. Transmission electron microscopy was used. We showed that the fibres were made of a microcrystallised silicon carbide phase. Diffracting areas were observed of sizes varying from 0.6 to 5 nm according to the fibre. Some fibres showed amorphous or turbostratic carbon segregations.
Résumé
Les propriétés d'un matériau composite dépendent à la fois de celles du renfort, de la matrice et de l'interface. Afin de contribuer à la caractérisation des composites céramiques SiC-SiC, nous avons étudié la microtexture de fibres de carbure de silicium (Nicalon) par des techniques de microscopie électronique par transmission. Nous avons montré que toutes les fibres présentent une phase de carbure de silicium microcristallisée. La taille des domaines diffractants varie de 0,6 à 5 nm selon la fibre. Certaines fibres présentent des ségrégations de carbone soit amorphe, soit turbostratique.
8120N - Preparation of cermets, ceramic and refractory composites.
Key words
ceramics -- composite material interfaces -- fibre reinforced composites -- silicon compounds -- transmission electron microscope examination of materials -- transmission electron microscopy -- fibres -- matrix -- interface properties -- amorphous -- turbostatic carbon segregations -- 0.6 to 5 nm -- ceramic composites SiC SiC -- SiC fibre reinforced SiC